> Try a wire brush followed by a generous douching with Osopho (phosporic
> acid). Then, blow off with air and paint primer on top of Osopho residue.
> Old oil field trick--works good, lasts long time.
>
I'm guessing Osopho is what Gavin and I know as Jenolite, if exfoliation has
started it doesn't hold it for long. The FV623 windscreen rebates had a
power wire brushing, Jenolite, red oxide and then NATO two-pack OD. Held it
for a year.